PVP
CROW logo
Poly(vinylpyrrolidone), PVP
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyetherketone
COMMON NAMESPoly(vinylpyrrolidone), Poly(N-vinylpyrrolidone),
STRUCTURE BASED NAME Poly(1-ethenylpyrrolidin-2-one)
ACRONYMS PVP
CAS # 9003-39-8
CurlySMILES C{-}C{n+}(N1CCCC1=O)
 

IDENTIFIERS OF MONOMER(S)

CAS #  
COMMON NAMESN-vinylpyrrolidone, 1-Ethenylpyrrolidin-2-one
SMILES C=CN1CCCC1=O
Std. InChI InChI=1S/C6H9NO/c1-2-7-5-3-4-6(7)8/h2H,1,3-5H2
Std. InChIKey WHNWPMSKXPGLAX-UHFFFAOYSA-N
STRUCTURE
Poly(ether ketone)
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1 85.5 - 10188.9
Density ρg mL-1 1.1 - 1.31.25
Solubility Parameter δMPa1/2 22.2 - 25.623.9
Molar Cohesive Energy EcohJ mol-1 45700 - 6110050800
Glass Transition Temperature TgK 438 - 448443
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone 1.53 - 1.571.55
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 111.14
Van-der-Waals Volume VvWmL mol-1 59.8
Molar Volume VmmL mol-1 83.984
Density ρg mL-1 1.32 1.32
Solubility Parameter δMPa1/2 22.3 - 24.3 24.3
Molar Cohesive Energy EcohJ mol-1 41800 - 4960049600
Glass Transition Temperature TgK 455 (?)
Molar Heat Capacity CpJ (mol K)-1 139 
Entanglement Molecular Weight Meg mol-1   
Index of Refraction n none 1.54

  Last updated: October 1, 2017

back to top