Poly(vinyl methyl ketone)
CROW logo
Poly(vinyl methyl ketone)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyvinylketones
COMMON NAMESPoly(vinyl methyl ketone)
STRUCTURE BASED NAME Poly(1-acetylethylene), Poly(methoylethylene)
ACRONYMS
CAS # 25038-87-3
CurlySMILES C{-}(C(=O)C)C{n+}
 

IDENTIFIERS OF MONOMER(S)

CAS # 78-94-4
COMMON NAMESVinyl methyl ketone
SMILES CC(=O)C=C
Std. InChI 1S/C4H6O/c1-3-4(2)5/h3H,1H2,2H3
Std. InChIKey FUSUHKVFWTUUBE-UHFFFAOYSA-N
STRUCTURE
Vinyl methyl ketone
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-162.6 - 67.062.6
Density ρg mL-1 1.05 - 1.121.12
Solubility Parameter δMPa1/2 19.3 - 22.920.7
Molar Cohesive Energy EcohJ mol-1 23300 - 3280026900
Glass Transition Temperature TgK 301
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone1.42 - 1.501.50
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 70.09
Van-der-Waals Volume VvWmL mol-1 42.06
Molar Volume VmmL mol-162.3 - 63.963.1
Density ρg mL-1 1.10 - 1.121.11
Solubility Parameter δMPa1/2 20.1 - 23.421.5
Molar Cohesive Energy EcohJ mol-1 25900 - 3460029300
Glass Transition Temperature TgK 305
Molar Heat Capacity CpJ (mol K)-193 - 101
141 - 146
97 (s)
142 (l,r)
Entanglement Molecular Weight Meg mol-14750 - 87007000
Index of Refraction nnone1.47 - 1.501.49