Poly(ethyl vinyl thioether)
CROW logo
Poly(ethyl vinyl thioether)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyvinylsulfide
COMMON NAMESPoly(ethyl vinyl thioether), Poly(vinyl ethyl sulfide)
STRUCTURE BASED NAME Poly(ethylthioethylene)
ACRONYMS
CAS #
CurlySMILES C{-}C{n+}(SCC)
 

IDENTIFIERS OF MONOMER(S)

CAS # 627-50-9
COMMON NAMESEthyl vinyl thioether, (Ethylthio)ethene, Ethyl Vinyl Sulfide
SMILES CCSC=C
Std. InChI 1S/C4H8S/c1-3-5-4-2/h3H,1,4H2,2H3
Std. InChIKey AFGACPRTZOCNIW-UHFFFAOYSA-N
STRUCTURE
Ethyl vinyl thioether
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1
Density ρg mL-1
Solubility Parameter δMPa1/2 22.1
Molar Cohesive Energy EcohJ mol-1 40200
Glass Transition Temperature TgK 266
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 88.17
Van-der-Waals Volume VvWmL mol-1 51.05
Molar Volume VmmL mol-180.3 - 83.982.4
Density ρg mL-1 1.05 - 1.101.07
Solubility Parameter δMPa1/2 17.5 - 18.217.8
Molar Cohesive Energy EcohJ mol-1 25500 - 2770026200
Glass Transition Temperature TgK 264 - 266265
Molar Heat Capacity CpJ (mol K)-1161 - 171165
Entanglement Molecular Weight Meg mol-17500 - 83008300
Index of Refraction nnone1.55 - 1.561.56
back to top