Poly(4-hydroxystyrene)
CROW logo
Poly(4-hydroxystyrene)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyvinylalcohol
COMMON NAMESPoly(4-hydroxystyrene), Poly(4-vinyl phenol)
STRUCTURE BASED NAME Poly[1-(4-hydroxyphenyl)ethane-1,2-diyl], Poly(4-hydroxyphenylethylene)
ACRONYMS PVP
CAS # 24979-70-2
CurlySMILES C{-}C{n+}(c1ccc(O)cc1)
 

IDENTIFIERS OF MONOMER(S)

CAS # 24979-70-2
COMMON NAMES4-Hydroxystyrene
SMILES C=Cc1ccc(cc1)O
Std. InChI 1S/C8H8O/c1-2-7-3-5-8(9)6-4-7/h2-6,9H,1H2
Std. InChIKey FUGYGGDSWSUORM-UHFFFAOYSA-N
STRUCTURE
4-Hydroxystyrene
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1103.6
Density ρg mL-1 1.16
Solubility Parameter δMPa1/2 22.5 - 24.623.6
Molar Cohesive Energy EcohJ mol-1 52400 - 6240057400
Glass Transition Temperature TgK 428 - 431, 473430, 473
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 120.15
Van-der-Waals Volume VvWmL mol-1 68.70
Molar Volume VmmL mol-1101.1 - 106.1103.6
Density ρg mL-1 1.13 - 1.191.16
Solubility Parameter δMPa1/2 23.4 - 24.824.0
Molar Cohesive Energy EcohJ mol-1 58000 - 6210059900
Glass Transition Temperature TgK 443, 494
Molar Heat Capacity CpJ (mol K)-1135 - 146140
Entanglement Molecular Weight Meg mol-124000 - 3000028000
Index of Refraction nnone1.611.61