Poly(hexyl cyanoacrylate)
CROW logo
Poly(hexyl cyanoacrylate)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polycyanoacrylates
COMMON NAMESPoly(hexyl cyanoacrylate)
STRUCTURE BASED NAME Poly(hexyl 2-cyanopropenoate), Poly(hexyl α-cyanoacrylate)
ACRONYMS
CAS #  
CurlySMILES C{-}C{n+}(C#N)(C(=O)OCCCCCC)
 

IDENTIFIERS OF MONOMER(S)

CAS #  
COMMON NAMESHexyl 2-cyanoacrylate
SMILES CCCCCCOC(=O)C(=C)C#N
Std. InChI 1S/C10H15NO2/c1-3-4-5-6-7-13-10(12)9(2)8-11/h2-7H2,1H3
Std. InChIKey XDZLHTBOHLGGCJ-UHFFFAOYSA-N
STRUCTURE
Poly(octyl cyanoacrylate)
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1
Density ρg mL-1
Solubility Parameter δMPa1/2   
Molar Cohesive Energy EcohJ mol-1
Glass Transition Temperature TgK 359 
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 181.24
Van-der-Waals Volume VvWmL mol-1 109.3
Molar Volume VmmL mol-1 161 - 165163
Density ρ g mL-1 1.10 - 1.121.11
Solubility Parameter δ MPa1/2 20.4 - 21.520.8
Molar Cohesive Energy Ecoh J mol-1 69000 - 7450070500
Glass Transition Temperature TgK 345 
Molar Heat Capacity CpJ (mol K)-1 260 - 276268 (s)
Entanglement Molecular Weight Meg mol-1   
Index of Refraction nnone 1.49 - 1.501.50