SHORE DUROMETER CONVERSION CHART

A B C D O
100 85 77 58
95 81 70 46
90 76 59 39
85 71 52 33
80 66 47 29 84
75 62 42 25 79
70 56 37 22 75
65 51 32 19 72
60 47 28 16 69
55 42 24 14 65
50 37 20 12 61
45 32 17 10 57
40 27 14 8 53
35 22 12 7 48
30 17 9 6 42
25 12 35
20 28
15 21
10   14
5   8